Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1574 Nomex FabricSide 2: Uncured SiliconeInterleave: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Interleave
63.5 microns
2.50 mil
Interleave
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
457 microns
18.0 mil
Side 2; Arlon SQA-TMS-003
914 microns
36.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
18.56 MPa
2692 psi
Fill; Arlon SQA-TMS-008
19.4 MPa
2810 psi
Warp; Arlon SQA-TMS-008
Elongation at Break 16 %
16 %
Warp; Arlon SQA-TMS-008
19 %
19 %
Fill; Arlon SQA-TMS-008
225 %
225 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
ASTM D624
Peel Strength 1.45 kN/m
8.30 pli
Bond Strength (S1 to S2); Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Copyright © lookpolymers.com All Rights Reserved