Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Side 2 Silicone Property; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Side 1 Silicone Property; Arlon SQA-TMS-024
Thickness 102 microns
4.00 mil
Side 1; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
965 microns
38.0 mil
Side 2; Arlon SQA-TMS-003
1520 microns
60.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Side 2 Silicone Property; ASTM D2240
52
52
Side 1 Silicone Property; ASTM D2240
Tensile Strength 6.14 MPa
890 psi
Side 1 Silicone Property; ASTM D412
7.58 MPa
1100 psi
Side 2 Silicone Property; ASTM D412
Elongation at Break 550 %
550 %
Side 1 Silicone Property; ASTM D412
650 %
650 %
Side 2 Silicone Property; ASTM D412
Peel Strength 5.47 kN/m
31.2 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 25.1 kV/mm
638 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 204 °C
4.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 60.1
Arlon SQA-TMS-025