Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.0 - 27 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.0 - 27 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 50-2000 Description: Utility Grade High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 23 - 27 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 - 27 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers NPP 50-2753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 23 - 27 g/10 min @Load 5.00 kg, Temperature 200 °C |
23 - 27 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D4153 E (O/E SBS) Linear Block Copolymer Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl.. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G1 EVA Film for Encapsulating Solar modules, Ultra Fast Cure EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G1/RF EVA Film for Encapsulating Solar modules, Reinforced Friendly EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemica.. |
|||
Melt Flow | 21 - 27 g/10 min @Load 5.00 kg, Temperature 372 °C |
21 - 27 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Melt Flow | 17 - 27 g/10 min @Load 21.6 kg, Temperature 150 °C |
17 - 27 g/10 min @Load 47.6 lb, Temperature 302 °F |
ISO 1133 |
Fainplast Compounds Hax™ HFC 0108/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 7846Information provided by Fainplast Compounds |
|||
Melt Flow | 21 - 27 g/10 min | 21 - 27 g/10 min | ASTM D1238 |
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Melt Flow | 17 - 27 g/10 min | 17 - 27 g/10 min | ASTM D1238 |
Lushan EV1050G2 EVA Film for Encapsulating Solar modules, High Transmittance EVA film for encapsulating solar modules Lushan EV1050G1 is mainly used for PV module encapsulation. It’s based on an ethylene vinyle acetate (EVA) copolymer and supplemented by special Chemical Ac.. |