Material Notes:
Description: Utility Grade High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.945 - 0.965 g/cc
0.0341 - 0.0349 lb/in³
ASTM D1505
Melt Flow 6.0 - 27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 - 27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.3 - 27.6 MPa
2800 - 4000 psi
ASTM D638
Elongation at Break 5.0 - 400 %
5.0 - 400 %
chs 2 in/min; ASTM D638
Flexural Modulus 0.862 - 1.21 GPa
125 - 175 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790