Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resistanceGood UV resistanceLow densityWide service range from -20°C to 120°CAppearance: BlackForms: Round or Strand Cut Gala PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.07 g/cc
1.02 - 1.07 g/cc
ASTM D792
Linear Mold Shrinkage 0.0065 - 0.0085 cm/cm
0.0065 - 0.0085 in/in
ASTM D955
Melt Flow 21 - 27 g/10 min
21 - 27 g/10 min
ASTM D1238
Ash 17 - 23 %
17 - 23 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
ASTM D2240
Tensile Strength, Yield >= 13.8 MPa
>= 2000 psi
ASTM D638
Flexural Modulus >= 0.951 GPa
>= 138 ksi
ASTM D790
Izod Impact, Notched >= 3.74 J/cm
>= 7.00 ft-lb/in
ASTM D256
Gardner Impact >= 271 J
>= 200 ft-lb
ASTM D5420