Physical Properties Metric English Comments
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 7150 BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 5.0 - 22 g/10 min

@Load 6.70 kg,
Temperature 337 °C
5.0 - 22 g/10 min

@Load 14.8 lb,
Temperature 639 °F
ASTM D1238
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Melt Flow 5.0 - 22 g/10 min

@Load 6.70 kg,
Temperature 337 °C
5.0 - 22 g/10 min

@Load 14.8 lb,
Temperature 639 °F
ASTM D1238
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Melt Flow 5.0 - 22 g/10 min

@Load 6.70 kg,
Temperature 337 °C
5.0 - 22 g/10 min

@Load 14.8 lb,
Temperature 639 °F
ASTM D1238
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
Melt Flow 6.0 - 22 g/10 min

@Load 6.70 kg,
Temperature 337 °C
6.0 - 22 g/10 min

@Load 14.8 lb,
Temperature 639 °F
ASTM D1238
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Melt Flow 10 - 22 g/10 min

@Load 0.325 kg,
Temperature 270 °C
10 - 22 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Melt Flow 17 - 22 g/10 min

@Load 2.16 kg,
Temperature 300 °C
17 - 22 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ISO 1133
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 18 - 22 g/10 min
18 - 22 g/10 min
ASTM D1238
Micropol L20 Low density polyethylene rotational molding powder
Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited
Melt Flow 18 - 22 g/10 min

@Load 2.16 kg,
Temperature 235 °C
18 - 22 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax CCP PBT 1100-630S
Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Melt Flow 18 - 22 g/10 min

@Load 2.16 kg,
Temperature 235 °C
18 - 22 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax PBT 1100-211M
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Melt Flow 18.1 - 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18.1 - 22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Iran Petrochemical (PCC) PC 1822 Polycarbonate
Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co.
Melt Flow 18 - 22 g/10 min

@Load 2.16 kg,
Temperature 240 °C
18 - 22 g/10 min

@Load 4.76 lb,
Temperature 464 °F
ASTM D1238
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang.
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 20 - 22 g/10 min
20 - 22 g/10 min
Cond. O
Ashley Polymers Ashlene® P1051R Polycarbonate
A high flow transparent polycarbonate with good impact properties.Data provided by the manufacturer
Melt Flow 20 - 22 g/10 min
20 - 22 g/10 min
Cond. O
Ashley Polymers Ashlene® P1053R Polycarbonate
A high flow transparent polycarbonate with good impact properties containing UV stabilizer.Data provided by the manufacturer