Ashley Polymers Ashlene® P1051R Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Optical Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P1051R Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high flow transparent polycarbonate with good impact properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Moisture Absorption at Equilibrium 0.34 %
0.34 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 20 - 22 g/10 min
20 - 22 g/10 min
Cond. O
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ATSM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Strength 95.0 MPa
13800 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Users viewing this material also viewed the following: