Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18 - 23 g/10 min | 18 - 23 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP1005M-EX8 PP Application: Polypropylene compound designed with halogen-based flame retardant technology meeting the UL 94 V-2 rating. Available in a wide range of colors and not subject to additive bloom.Info.. |
|||
Melt Flow | 17 - 23 g/10 min | 17 - 23 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-61/CC/40 Polypropylene Copolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 18 - 23 g/10 min | 18 - 23 g/10 min | ASTM D1238 |
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H20SLME Polypropylene Homopolymer This is a homopolymer designed for injection molding, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H20YLME Polypropylene Homopolymer This is a homopolymer designed for injection molding, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem HA 7260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 15 - 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 - 23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Kraton® G1726 M (SEBS) Linear Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 7.0 - 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 - 23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 280 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 536 °F |
Z-011A |
Zeon Chemicals Zeonex® 480 Cyclo-Olefin Polymer |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1467-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1467-01ApplicationPP 1467-01 meet FDA Regulation 21 CFR 177.1520, for all food contact applications.Information provided by A. Schulman. |
|||
Melt Flow | 17 - 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
17 - 23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H20BLME Polypropylene Homopolymer This is a homopolymer designed for injection molding, and it is compliant with both the FDA status and the EU Food Contact status.Information provided by Ineos Olefins & Polymers USA |
|||
Melt Flow | 15 - 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 - 23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Kraton® G1726 M (SEBS) Linear Triblock Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |