Fiberfil® PP-61/CC/40 Polypropylene Copolymer, 40% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer FiberFil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® PP-61/CC/40 Polypropylene Copolymer, 40% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 17 - 23 g/10 min
17 - 23 g/10 min
230/2.16 (typical); ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.00 MPa
2465 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm
1.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C
133 °F
ASTM D648