Physical Properties Metric English Comments
Melt Flow 0.700 - 53.5 g/10 min
0.700 - 53.5 g/10 min
Average value: 18.2 g/10 min Grade Count:66
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Melt Flow 0.700 - 230 g/10 min
0.700 - 230 g/10 min
Average value: 13.1 g/10 min Grade Count:106
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Melt Flow 0.700 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.700 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2327-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 0.700 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.700 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-86-K975-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 0.700 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.700 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-88-N809C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.700 - 110 g/10 min
0.700 - 110 g/10 min
Average value: 32.7 g/10 min Grade Count:15
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Melt Flow 0.700 - 20.0 g/10 min
0.700 - 20.0 g/10 min
Average value: 2.83 g/10 min Grade Count:46
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
Melt Flow 0.700 - 14.0 g/10 min
0.700 - 14.0 g/10 min
Average value: 3.43 g/10 min Grade Count:27
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Melt Flow 0.700 - 16.0 g/10 min
0.700 - 16.0 g/10 min
Average value: 4.18 g/10 min Grade Count:124
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Melt Flow 0.700 - 40.0 g/10 min
0.700 - 40.0 g/10 min
Average value: 10.7 g/10 min Grade Count:131
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..