Polymer Property : Melt Flow = 0.900 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.900 - 99.0 g/10 min
0.900 - 99.0 g/10 min
Average value: 8.02 g/10 min Grade Count:409
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Melt Flow 0.900 - 16.9 g/10 min
0.900 - 16.9 g/10 min
Average value: 7.80 g/10 min Grade Count:3
Overview of materials for Polycarbonate, Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr..
Melt Flow 0.900 - 19.0 g/10 min
0.900 - 19.0 g/10 min
Average value: 3.77 g/10 min Grade Count:17
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Melt Flow 0.900 - 70.0 g/10 min
0.900 - 70.0 g/10 min
Average value: 13.9 g/10 min Grade Count:61
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Melt Flow 0.900 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.900 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer
Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;..
Melt Flow 0.900 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.900 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.900 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.900 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.900 - 16.0 g/10 min
0.900 - 16.0 g/10 min
Average value: 7.14 g/10 min Grade Count:17
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Copyright © lookpolymers.com All Rights Reserved