ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: LV silane cross-linking insulation – 2 step processInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.931 g/cc
0.0336 lb/in³
ExxonMobil method
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D638
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 510 %
510 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 379 MPa
55000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 241 °C
<= 466 °F
Peak Melting Point; ExxonMobil method
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
ASTM D257
Dielectric Constant 2.2

@Frequency 60.0 Hz
2.2

@Frequency 60.0 Hz
STM D150
Dielectric Strength 63.0 kV/mm
1600 kV/in
50 V/sec; ASTM D149
Dissipation Factor 0.0010

@Frequency 60.0 Hz
0.0010

@Frequency 60.0 Hz
ASTM D150
Users viewing this material also viewed the following: