Ineos B4020N1331 Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos B4020N1331 Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, this grade is certified as low taste and is intended for packaging in direct contact with beverages. It has a broad molecular weight distribution for faster molding cycles and enhanced stress crack resistance. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.Typical ApplicationsCaps and closures for the packaging of sparkling water or carbonated beveragesInjection and compression molded applications where low taste and odor are criticalInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 10 hour
10 hour
Condition B, 10%; ASTM D1693
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 28.3 MPa
4100 psi
2 in/min; ASTM D638
Elongation at Break >= 700 %
>= 700 %
2 in/min; ASTM D638
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Tangent Modulus 1170 MPa
170000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.8 °C
154 °F
ASTM D648
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746