Material Notes:
D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended for use in extrusion blow molding, sheet extrusion, and thermoforming processes where enhanced clarity and weatherability is desired.Information provided by Dow
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 1.9 g/10 min

@Temperature 230 °C
1.9 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
1% Secant; ASTM D790A
Izod Impact, Notched 2.94 J/cm
5.50 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
unannealed; ASTM D648