Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.20 - 150 g/10 min | 1.20 - 150 g/10 min | Average value: 39.0 g/10 min Grade Count:49 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Melt Flow | 1.20 - 100 g/10 min | 1.20 - 100 g/10 min | Average value: 9.36 g/10 min Grade Count:116 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Melt Flow | 1.20 - 2.60 g/10 min | 1.20 - 2.60 g/10 min | Average value: 2.08 g/10 min Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 1.20 - 162 g/10 min | 1.20 - 162 g/10 min | Average value: 46.6 g/10 min Grade Count:15 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Melt Flow | 1.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4675A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 1.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4755A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 1.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1017A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 1.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Melt Flow | 1.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-150 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Melt Flow | 1.20 - 2.00 g/10 min | 1.20 - 2.00 g/10 min | Average value: 1.80 g/10 min Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 1.20 - 45.0 g/10 min | 1.20 - 45.0 g/10 min | Average value: 13.5 g/10 min Grade Count:24 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |