Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.20 - 162 g/10 min | 1.20 - 162 g/10 min | Average value: 46.6 g/10 min Grade Count:15 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |