Polymer Property : Melt Flow = 2.00 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.00 - 2.00 g/10 min
1.00 - 2.00 g/10 min
Average value: 1.81 g/10 min Grade Count:10
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Melt Flow 1.20 - 2.00 g/10 min
1.20 - 2.00 g/10 min
Average value: 1.80 g/10 min Grade Count:4
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max..