Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global G-2855 High Density Polyethylene, Blow Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global G-2855 High Density Polyethylene, Blow Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in food additives regulations 21 CFR 177.1520 for use in direct contact with food.Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 36.0 MPa
5220 psi
ASTM D638
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 2000 %
2000 %
ASTM D638
Users viewing this material also viewed the following: