Physical Properties Metric English Comments
Viscosity 7500 cP
7500 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive
Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to ..
Viscosity 7500 cP

@Temperature 175 °C
7500 cP

@Temperature 347 °F
Automatic orifice Viscosity
Cookson Group Plaskon® LS-16S Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress molding compound specifically formulated for use with conventional molding equipment to increase semiconductor manuf..
Viscosity 7500 cP

@Temperature 175 °C
7500 cP

@Temperature 347 °F
Automatic orifice Viscosity
Cookson Group Plaskon® AMC2 (132.203) Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound specifically formulated for packaging stress-sensitive devices in DIPs, SOICs, PLCCs and small QFPs. F..
Viscosity 7500 - 9500 cP
7500 - 9500 cP
Huntsman Araldite GY 6005 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 182 to 196. Max color is 1.Comments/Applications: Slightly modified GY 6010. Medium viscosity, general purpose, highly versatile resin for use in cold or heat-cured ..
Viscosity 7500 - 9500 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
7500 - 9500 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2050926P2 Lead-free Ag PZT Paste
This product is a Lead free termination for single layer PZT ceramics. After firing the film has good adhesion and solderability. Screen Printing Equipment: semi-automatic, manualScreen Types: stai..
Viscosity 7500 - 11000 cP
7500 - 11000 cP
Lucite International Colacryl ® 1207 Acrylic Solution Resin
A soft and flexible resin produced in a slow drying ester and designed for printing inks and covercoats on ceramic and glass transfers. The product is compatible with common drying and non-drying lo..
Viscosity 7500 - 15000 cP
7500 - 15000 cP
#3 SP @ 6 rpm
Solvay MACKERNIUM® 007N Surfactant
Product Description: Mackernium 007N is an aqueous solution of a positively charged copolymer of diallyldimethylammonium chloride and acrylamide with a molecular weight of approximately 2,000,000. I..
Viscosity <= 7500 cP
<= 7500 cP
#4 SP @ 10 rpm; RP-0659
Solvay MIRACARE® PLAISANT Surfactant
Description: This is a plant-based system for cleansing cosmetics. Ultra mild, with excellent foam volume and lather characteristics, it is compatible with anionic, nonionic and amphoteric surfactan..
Viscosity <= 7500 cP
<= 7500 cP
#3 SP @ 6 rpm; RP-0596
Solvay MIRACARE® TSC 484 Surfactant
Description: Miracare TSC 484 is a fully formulated Performance Concentrate. It is designed as an economical alternative to SLS, SLES, and Lauryl based blends. It has similar viscosity building prop..
Viscosity 7500 - 15000 cP
7500 - 15000 cP
540MA3C52
Solvay MIRAPOL® 550 P Surfactant
Description: Mirapol 550 P can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to provide excellent lubricity, softeness light hair conditioning and..
Viscosity 7500 - 15000 cP
7500 - 15000 cP
#4 SP @ 10 rpm; RP-0596
Solvay MIRAPOL® 550 Surfactant
Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, anti-static, luster and detangling properties to the hair and silky feel to the skin. Stabilizes foa..
Viscosity 7500 cP
7500 cP
Part A
Loctite® 3035™ Polyolefin Bonder
Loctite® 3035™ Polyolefin Bonder is an easy-to-use, 1:1 mix product that can be stored at room temperature and works where traditional low surface energy bonders often fail. Loctite® 3035™ Polyo..
Viscosity 7500 cP
7500 cP
Dynamic
Dow Corning 3581 Performance Modifier
Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning
Viscosity 7500 cP
7500 cP
catalyzed with QM CAT RED 3
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us..
Viscosity 7500 cP
7500 cP
catalyzed with QM CAT BLUE
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us..
Viscosity 7500 cP
7500 cP
catalyzed with QM CAT PURPLE
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us..
Viscosity 7500 cP
7500 cP
Base
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
Viscosity >= 7500 cP
>= 7500 cP
Accelerator
3M Scotch-Weld™ DP807 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Viscosity >= 7500 cP
>= 7500 cP
Accelerator
3M Scotch-Weld™ DP812 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Viscosity >= 7500 cP
>= 7500 cP
Accelerator
3M Scotch-Weld™ DP825 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and..
Viscosity 7500 cP
7500 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive
Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m..
Viscosity 7500 cP
7500 cP
Mixed; TM R050-12
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin
Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula..