Material Notes:
Description: Cationic polymer providing good wet/dry combability properties. Imparts smooth feel, anti-static, luster and detangling properties to the hair and silky feel to the skin. Stabilizes foam while providing richness. Stable over a wide pH range.Chemical Name: AQUEOUS CATIONIC COPOLYMERCAS: 26590-05-6 I.N.C.I. Name: POLYQUATERNIUM-7 Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in waterUse level: 0.2-5%Applications: MIRAPOL® 550 can be used effectively in shampoos and conditioners at typical use levels of 0.5% (copolymer solids) to impart excellent gloss, lubricity, softness and combability improvements to hair without excessive build-up. At higher concentrations the film forming attributes of MIRAPOL 550 may be utilized in hair gels, mousses and setting lotions. Skin care applications include shaving creams, bath additives, creams, lotions and deodorants. MIRAPOL® 550 can be dispersed in water with agitationInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 8.0 - 9.0 %

@Temperature 150 °C,
Time 3600 sec
8.0 - 9.0 %

@Temperature 302 °F,
Time 1.00 hour
Oven; RP-0823
pH 6.5 - 7.5
6.5 - 7.5
RP-0420
Viscosity 7500 - 15000 cP
7500 - 15000 cP
#4 SP @ 10 rpm; RP-0596
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear, Colorless Viscous Solution
RP-0064
Color <70
APHA,RP-0134
Composition Phenonip
0.001
Residual acrylamide
<10 ppm, RP-0764