Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 45000 - 65000 cP @Temperature 40.0 °C |
45000 - 65000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 30000 - 65000 cP | 30000 - 65000 cP | mixed compound; thixotropic |
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
Viscosity | 50000 - 65000 cP | 50000 - 65000 cP | Part B |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |