Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 65000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 45000 - 65000 cP

@Temperature 40.0 °C
45000 - 65000 cP

@Temperature 104 °F
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Viscosity 30000 - 65000 cP
30000 - 65000 cP
mixed compound; thixotropic
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy
Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun..
Viscosity 50000 - 65000 cP
50000 - 65000 cP
Part B
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System
Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t..
Copyright © lookpolymers.com All Rights Reserved