Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 45000 - 65000 cP

@Temperature 40.0 °C
45000 - 65000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82
78 - 82
Tensile Strength at Break 28.44 - 42.17 MPa
4125 - 6116 psi
Elongation at Break 545 - 645 %
545 - 645 %
Tear Strength 63.7 - 103 kN/m
364 - 588 pli
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 12 min
12 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 3%
Min 2.6%
PHR of MOCA 8.3%