Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to .. |
|||
Viscosity | 30000 - 65000 cP | 30000 - 65000 cP | mixed compound; thixotropic |
Master Bond EP112FLAN-1 Two Component Flexibilized Heat Curing Epoxy Master Bond EP112FLAN-1 is a toughened two component, high performance epoxy resin system featuring good temperature resistance, high thermal conductivity, fine electrical insulation values and soun.. |
|||
Viscosity | 30000 - 70000 cP | 30000 - 70000 cP | Part A |
Master Bond EP33CLV Epoxy Resists Chemicals and High Temperatures Description: Master Bond EP33CLV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and excel.. |
|||
Viscosity | 30000 cP @Temperature 25.0 °C |
30000 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid.. |
|||
Viscosity | 30000 cP @Temperature 25.0 °C |
30000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 2741LV/15LV Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Viscosity | 30000 cP | 30000 cP | Part A at 20 RPM |
Loctite® 3273 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 30000 - 40000 cP @Temperature 23.0 °C |
30000 - 40000 cP @Temperature 73.4 °F |
|
Master Bond Supreme 11 High Peel and Shear Strength Epoxy Adhesive Master Bond Polymer System Supreme 11 features a unique balance of performance properties including both high shear and high peel strengths. This two component adhesive system is formulated to cure .. |
|||
Viscosity | 30000 cP | 30000 cP | Mixed - high; Resin - nonsag paste; Hardener - 30,000 cP |
Loctite® Durabond® E-20NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Viscosity | 30000 cP | 30000 cP | Dynamic |
Dow Corning 7-3101 Elastomer Blend Hip Emulsion A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollient.. |
|||
Viscosity | 30000 cP | 30000 cP | Dynamic |
Dow Corning 7-3118 EBAP Hip Emulsion A concentrated emulsion of dimethicone crosspolymer in cyclopentasiloxane and dimethicone that is designed to facilitate the rapid development of skin care formulations which contain these emollient.. |
|||
Viscosity | 30000 - 80000 cP | 30000 - 80000 cP | dynamic |
Dow Corning Q2-7735 ADHESIVE Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning |
|||
Viscosity | 30000 cP | 30000 cP | |
Epoxyset Epoxiohm EO-21 Electrically Conductive Epoxy Adhesive EO-21 is a two part, silver filled high electrical conductivity epoxy adhesive. It is designed to cure at room temperature or rapidly at elevated temperature and exhibits very excellent adhesion and.. |
|||
Viscosity | >= 30000 cP | >= 30000 cP | |
Epoxyset Epoxiohm EO-30M-1 Electrically Conductive Epoxy Adhesive EO-30M-1 is a two part, semi-rigid, silver filled, epoxy adhesive. EO-30M-1 exhibits superior adhesion to a wide variety of substrates including most metals, ceramics, glass and plastics.Information.. |
|||
Viscosity | 30000 - 35000 cP | 30000 - 35000 cP | |
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl.. |
|||
Viscosity | 30000 cP | 30000 cP | |
Dymax 3073 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 30000 cP | 30000 cP | Thixotropic Gel |
Dymax EMAX 10002 Voil Coil Assembly Disk Drive Adhesive Disk Drive AdhesivesLow Outgassing Multi-Cure® Memory Saver Disk Drive AdhesivesDescriptionDymax offers a range of advanced formula epoxy and acrylic adhesives for disk drive assembly. UV cures in .. |
|||
Viscosity | 30000 cP | 30000 cP | |
ACC MM239 Addition Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: ceramic/polyester/PU/epoxy a.. |
|||
Viscosity | 30000 cP | 30000 cP | |
ACC MM922 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM 245B |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT SKIN 30 |
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT RED 3 |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 30000 cP | 30000 cP | catalyzed with QM CAT BLUE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Viscosity | 30000 cP | 30000 cP | |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Viscosity | 30000 cP | 30000 cP | |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Viscosity | 30000 - 70000 cP | 30000 - 70000 cP | Accelerator |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Viscosity | 30000 - 100000 cP | 30000 - 100000 cP | Thixotropic |
Loctite® 574 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps |
|||
Viscosity | 30000 cP | 30000 cP | Mixed; TM R050-12 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |