Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support systems for membrane-based immunodiagnostic tests.The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 43 - 47 %
43 - 47 %
Viscosity 1700 - 1900 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
1700 - 1900 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature >= 5.00 °C
>= 41.0 °F
cool dry place
Processing Properties Metric English Comments
Processing Temperature 40.0 °C
104 °F
70.0 - 80.0 °C
158 - 176 °F
activation temperature used to laminate with a press or vacuum tube
Cure Time 15 - 30 min
0.25 - 0.5 hour
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage m2/ltr 12