Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.022 - 0.026 cm/cm
0.022 - 0.026 in/in
ASTM D955
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
Annealed; ISO 294-4
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
ASTM D955
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement  (discontinued *
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
ISO 294
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer
INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info..
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
ISO 294
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer
INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide..
Linear Mold Shrinkage, Transverse 0.022 - 0.0245 cm/cm
0.022 - 0.0245 in/in
LATI Latilub 73/13-20T POM, PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Thickness 3.20 mm
0.022 in/in

@Thickness 0.126 in
Unitika A125 PA66, Conditioned
Information provided by Unitika Ltd.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Thickness 3.20 mm
0.022 in/in

@Thickness 0.126 in
Unitika A125 PA66, Dry
Information provided by Unitika Ltd.
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
Sim. To ISO 294-4
DSM Novamid® 3010SR NAT PA66
Easy Molding Grade
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
ISO 294-4
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
ISO 294-4
DSM Stanyl® TS272A1 PA46-RF
Aramid fiber reinforced, Wear and Friction Modified
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Thickness 2.00 mm
0.022 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® S600LF NC010 PBT
Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.022 cm/cm
0.022 in/in
Sheet; ISO 294
BASF Ultradur® B 6550 LN PBT
Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF