Linear Mold Shrinkage, Transverse 0.022 - 0.0245 cm/cm
0.022 - 0.0245 in/in
LATI Latilub 73/13-20T POM, PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..