Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.022 - 0.026 cm/cm | 0.022 - 0.026 in/in | ASTM D955 |
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | ASTM D955 |
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement
(discontinued * Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-9000 MA N Polypropylene Copolymer INNOPOL® CS 2-9000 MA N is a high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA N is developed for producing injection molded automotive components.All information provide.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 - 0.0245 cm/cm | 0.022 - 0.0245 in/in | |
LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
Unitika A125 PA66, Conditioned Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Thickness 3.20 mm |
0.022 in/in @Thickness 0.126 in |
|
Unitika A125 PA66, Dry Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | Sim. To ISO 294-4 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | ISO 294-4 |
DSM Novamid® ST145 NAT PA6-I Impact Modified, Injection Molding |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | ISO 294-4 |
DSM Stanyl® TS272A1 PA46-RF Aramid fiber reinforced, Wear and Friction Modified |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Thickness 2.00 mm |
0.022 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm | 0.022 in/in | Sheet; ISO 294 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |