Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick.Availability:Asia PacificEuropeNorth America Additive:HalogenLubricant Features:DuctileFlame RetardantGood Crack ResistanceGood Mold ReleaseGood ToughnessHalogenatedHigh ElongationIgnition ResistantLow DensityLubricatedUses:AppliancesAutomotive ElectronicsBobbinsConnectorsElectrical HousingElectrical PartsElectrical/Electronic ApplicationsFastenersIndustrial ApplicationsLighting ApplicationsLiving HingesPrinted Circuit BoardsSwitchesAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.9 %
1.9 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Diameter 2.00 mm
0.013 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527-2
Elongation at Break 75 %
75 %
ISO 527-2
Elongation at Yield 25 %
25 %
ISO 527-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-2
Flexural Strength 43.0 MPa
6240 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178