Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00190 - 0.0100 cm/cm
0.00190 - 0.0100 in/in
Average value: 0.00715 cm/cm Grade Count:10
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Linear Mold Shrinkage, Transverse 0.00190 - 0.0110 cm/cm
0.00190 - 0.0110 in/in
Average value: 0.00698 cm/cm Grade Count:5
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..