Teknor Apex APEX® 84132 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 84132 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 80°C Insulation and Jacketing; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 seconds; ASTM D2240
Tensile Strength at Break 17.4 MPa
2530 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -30.0 °C
-22.0 °F
ASTM D746
Oxygen Index 29 %
29 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+13 ohm-cm

@Temperature 50.0 °C
1.20e+13 ohm-cm

@Temperature 122 °F
ASTM D257
Descriptive Properties Value Comments
Appearance Opaque