Polymer Property : Specific Gravity = 1.07 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.07 g/cc
1.04 - 1.07 g/cc
ASTM D792
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® DigiGuard® Gloss 100 Water based overprint varnish
Description: Water based overprint varnishUsage: DigiGuard® Gloss 100 is a heat resistant, glossy overprint varnishFood Contact Information when manufactured in the USA:FDA: 175.105: Components o..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® Licomer® A 41 Styrene-Acrylate copolymer dispersion
Description: Styrene-Acrylate copolymer dispersionUsage: Licomer® A 41 is an aqueous polymer dispersion for dry bright emulsions for household floors, shoes and leather products to provide high g..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® Licomer® M 36 Styrene-Acrylate copolymer dispersion
Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 36 is suitable for easy removal dry-bright emulsions and provides a film with good resistance to alcohol.Info..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® ThermaGloss® 419 Water based over print varnish
Description: Water based over print varnish.Usage: Thermals® 419 is a high heat resistant overprint which imparts excellent gloss to preprinted linerboard while eliminating picking and smearing o..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® ThermaGloss® 420 Water based over print varnish
Description: Water based over print varnish.Usage: ThermaGloss® 420 is a high heat resistant overprint which imparts excellent gloss to preprinted liner board while eliminating picking and smeari..
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
Michelman® ThermaGloss® 426 Water based over print varnish
Description: Water based overprint varnish.Usage: ThermaGloss® 426 is a high heat resistant overprint which imparts excellent gloss to preprinted linerboard while eliminating picking and smearing..
Specific Gravity 1.02 - 1.07 g/cc
1.02 - 1.07 g/cc
ASTM D792
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Specific Gravity 1.04 - 1.07 g/cc
1.04 - 1.07 g/cc
ASTM D792
Buckeye Polymers BP RPP 2009 GK (B) BLK Polypropylene, 20% Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..