Michelman® ThermaGloss® 419 Water based over print varnish

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name ThermaGloss®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® ThermaGloss® 419 Water based over print varnish.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Water based over print varnish.Usage: Thermals® 419 is a high heat resistant overprint which imparts excellent gloss to preprinted linerboard while eliminating picking and smearing of the inks through the hot plate section of the corrugator. ThermaGloss® 419 has a reduced angle of skid. ThermaGloss® 419 is not gluable.Application Data: ThermaGloss® 419 is designed for application by flexo or gravure on a preprint press.Typical uses include: Retail packaging; POP displays; and Ink protectionFood Contact Information when manufactured in the USA: FDA: 175.105: Components of adhesives.176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.07 g/cc
1.05 - 1.07 g/cc
pH 8.3 - 9.3
8.3 - 9.3
Brookfield Viscosity 50 - 200 cP
50 - 200 cP
Spindle # 3, rpm 60
Viscosity Measurement 21 - 30
21 - 30
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance Light tan liquid
Solids Type Polymer