Material Notes:
Dow Corning® Z-6030 Silane is a bifunctional silane containing a methacrylate reactive organic group and a trimethoxysilyl inorganic group. The product is designated ?- methacryloxypropyltrimethoxysilane. Dow Corning® Z-6030 Silane possesses both organic and inorganic reactivity, reacting with organic thermoset resins as well as inorganic minerals such as glass and silica. The chemical bonding at the organic/inorganic interface that can occur with organofunctional silanes provides a variety of benefits listed above. Dow Corning® Z-6030 Silane is one of a series of Dow Corning organo functional silane chemicals. Other reactive silanes include the amine (Dow Corning® Z-6020 Silane), epoxy (Dow Corning® Z-6040 Silane), vinyl Dow Corning® Z-6300 Silane) and chloroalkyl (Dow Corning® Z-6076 Silane).Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc

@Temperature 25.0 °C
1.04 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 2.5 cSt
2.5 cSt
Molecular Weight 248.35 g/mol
248.35 g/mol
Thermal Properties Metric English Comments
Boiling Point 190 °C
374 °F
Flash Point 138 °C
280 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.43
1.43
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance clear
Color light straw, white
Purity (%) 98
Water Resistant yes