Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Load 10.0 kg,
Temperature 220 °C
1.3 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
chs 2 in/min; ASTM D638
Flexural Modulus 1.867 GPa
270.8 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 3.42 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
6.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 116 °C

@Load 1.00 kg,
Thickness 3.17 mm
241 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Optical Properties Metric English Comments
Gloss 96.7 %
96.7 %
60°; ASTM D523