Network Polymers SBN 150 Styrene Butadiene Acrylonitrile Terpolymer

Category Polymer , Thermoplastic , Acrylic (PMMA) , Polystyrene (PS) , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers SBN 150 Styrene Butadiene Acrylonitrile Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Styrene Butadiene Acrylonitrile TerpolymerInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 7.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.5 MPa
6600 psi
2 in per min; ASTM D638
Elongation at Break 10 %
10 %
chs 2 in/min; ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
Tangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
0.125 inch bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °C
181 °F
0.125 inch bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 99.0 °C
210 °F
0.125 inch bar, 1 Kg; ASTM D1525