Material Notes:
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.017 cm/cm

@Thickness 3.17 mm
0.017 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 0.20 g/10 min

@Load 1.00 kg,
Temperature 235 °C
0.20 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
1.9 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.9 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Instantaneous; ASTM D2240
Tensile Strength, Yield 6.14 MPa
890 psi
chs 20 in/min; ASTM D412
Elongation at Break 1000 %
1000 %
ASTM D412
Tear Strength 27.5 kN/m
157 pli
ASTM D624