Material Notes:
Description: Kraton D1160 E is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from Europe in the physical form identified: D1160 ES - supplied as porous pellets dusted with silicaD1160 EU - supplied as undusted porous pelletsRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1160 E is used in formulating adhesives, in particular hot melt pressure sensitive adhesives.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ISO 2781
Bulk Density 0.350 g/cc
0.0126 lb/in³
ASTM D1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Brookfield Viscosity 1000 cP
1000 cP
25% Toluene Solution at 25°C; KM 06
Molecular Weight 168000 - 188000 g/mol
168000 - 188000 g/mol
KM 01
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash 0.10 - 0.40 %
0.10 - 0.40 %
S; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 48

@Time 30.0 sec
48

@Time 0.00833 hour
ISO 868
Tensile Strength 32.0 MPa
4640 psi
ISO 37
Elongation at Break 1300 %
1300 %
ISO 37
300% Modulus 0.000190 GPa
0.0276 ksi
ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.06%, primary phenolic antioxidant, KM 08
Polystyrene
17.4-20.5%, KM 03
Total Extractables
<1.0%, KM 05