Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.760 g/cc | 0.760 g/cc | ASTM D792 |
S&E Specialty Polymers TufLite™ GT-11-030-B3 PVC Application: Expandable PVC footwear compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 0.760 g/cc | 0.760 g/cc | |
Parker Chomerics Tecknit® 239 Primer Typical Applications: Primer for TECKNIT 0192 & 0193Information provided by Chomerics |
|||
Specific Gravity | 0.760 - 0.780 g/cc | 0.760 - 0.780 g/cc | |
Michelman® Mold Release 225SS Synthetic wax emulsion Description: Solvent based, synthetic wax emulsionUsage: Mold Release 225SS is a solvent based mold release agent suitable for use with ceramics.Information provided by Michelman® |
|||
Specific Gravity | 0.760 g/cc @Temperature 25.0 °C |
0.760 g/cc @Temperature 77.0 °F |
|
Dow Corning OS-10 Information provided by Dow Corning |
|||
Specific Gravity | 0.760 g/cc @Temperature 25.0 °C |
0.760 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200, 0.65CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID .65CS. A volatile siloxane fluid (hexamethyldisiloxane).Information provided by Dow Corning |
|||
Specific Gravity | 0.760 g/cc @Temperature 25.0 °C |
0.760 g/cc @Temperature 77.0 °F |
|
Dow Corning 200® 0.65 CST FLUID Volatile siloxane fluid (hexamethyldisiloxane).Information provided by Dow Corning |
|||
Specific Gravity | 0.760 g/cc | 0.760 g/cc | ASTM-D-792-66 |
BCC Products EB 6200 Epoxy Tooling Board EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected.. |