S&E Specialty Polymers TufLite™ GT-11-030-B3 PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufLite™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufLite™ GT-11-030-B3 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Expandable PVC footwear compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.760 g/cc
0.760 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 46.0

@Time 15.0 sec
46.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 2.96 MPa
429 psi
ASTM D412
Elongation at Break 240 %
240 %
ASTM D412