Dow Corning 200® 0.65 CST FLUID

Category Fluid
Manufacturer Dow Corning
Trade Name 200®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 200® 0.65 CST FLUID.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Volatile siloxane fluid (hexamethyldisiloxane).Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.760 g/cc

@Temperature 25.0 °C
0.760 g/cc

@Temperature 77.0 °F
Viscosity Measure 0.65 cSt
0.65 cSt
kinetic/kinematic
Surface Tension 15.9 dynes/cm
15.9 dynes/cm
Thermal Properties Metric English Comments
Boiling Point 100 °C
212 °F
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flash Point -3.00 °C
26.6 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.375
1.375
Descriptive Properties Value Comments
Appearance clear
Hydrophobic yes