Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.760 - 0.780 g/cc | 0.760 - 0.780 g/cc | |
Michelman® Mold Release 225SS Synthetic wax emulsion Description: Solvent based, synthetic wax emulsionUsage: Mold Release 225SS is a solvent based mold release agent suitable for use with ceramics.Information provided by Michelman® |