Polymer Property : Specific Gravity = 0.780 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.760 - 0.780 g/cc
0.760 - 0.780 g/cc
Michelman® Mold Release 225SS Synthetic wax emulsion
Description: Solvent based, synthetic wax emulsionUsage: Mold Release 225SS is a solvent based mold release agent suitable for use with ceramics.Information provided by Michelman®