Material Notes:
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm

@Thickness 3.17 mm
0.016 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength 37.9 MPa
5500 psi
ASTM D638
Elongation at Yield 130 %
130 %
ASTM D638
Flexural Yield Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Thickness 3.17 mm
16.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 86.4 µm/m-°C
48.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Dielectric Strength 15.7 kV/mm
400 kV/in
Method A (Short-Time); ASTM D149