Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Viscosity 1.40e+6 cP
1.40e+6 cP
B
1.70e+6 cP
1.70e+6 cP
A
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 5.0
5.0
Tensile Strength 2.10 MPa
305 psi
Elongation at Yield 870 %
870 %
100% Modulus 0.000152 GPa
0.0220 ksi
Tear Strength 9.00 kN/m
51.4 pli
Compression Set 30 %

@Temperature 150 °C,
Time 3600 sec
30 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 28
T10 (302°F, ODR)
47
T90 (302°F, ODR)