Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Viscosity 800000 cP
800000 cP
B
1.30e+6 cP
1.30e+6 cP
A
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 9.0
9.0
Tensile Strength 2.80 MPa
406 psi
Elongation at Yield 580 %
580 %
100% Modulus 0.000179 GPa
0.0260 ksi
Tear Strength 10.0 kN/m
57.1 pli
Compression Set 22 %

@Temperature 150 °C,
Time 3600 sec
22 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 24
T10 (302°F, ODR)
51
T90 (302°F, ODR)
Copyright © lookpolymers.com All Rights Reserved