Solvay Engineered Polymers SEQUEL® 1820 Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1820 Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1820 engineered polyolefin is designed for automotive exterior applications that require energy management combined with excellent ductility and stiffness over a broad temperature range. This material provides excellent processability and dimensional stability. Applications: Body panels, bumper beams, energy absorbers, and brackets. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
after bake; ISO 294
Melt Flow 14 g/10 min
14 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 2.30 GPa
334 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 20.0 J
14.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
27.8 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Users viewing this material also viewed the following: