Material Notes:
3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler loadings; improve hardness; and add burnish, scrub and abrasion resistance to a variety of coating formulations. Due to the ceramic chemistry of these products, they are also UV transparent down to 250 nm and have utility in radiation-curable and thin-film powder coatings.Information provided by 3M
Physical Properties Metric English Comments
Bulk Density 1.50 g/cc
0.0542 lb/in³
Density 2.40 g/cc
0.0867 lb/in³
Particle Size 1.0 µm
1.0 µm
10" Percentile
3.0 µm
3.0 µm
50" Percentile
9.0 µm
9.0 µm
90" Percentile
12 µm
12 µm
95" Percentile
pH 9.0 - 12
9.0 - 12
ASTM E70
Specific Surface Area 5.0 m²/g
5.0 m²/g
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0
6.0
Compressive Strength >= 414 MPa
>= 60000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 2.30 W/m-K
16.0 BTU-in/hr-ft²-°F
Softening Point 1020 °C
1870 °F
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
Predominat, Becke Line
Electrical Properties Metric English Comments
Dielectric Constant 3.19
3.19
Descriptive Properties Value Comments
Color White
Oil Absorption 46 gm oil/100cc microspheres
Whiteness 95
Hunter, "L" Value, ASTM D2244