Material Notes:
Higher N, O, Fe contentsHot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in production of Al in Hall-Heroult cellsHot pressed TiB, armor platesCutting tools and cermets, suitable for machining aluminumMetal Matrix Composites
Physical Properties Metric English Comments
Particle Size 3.0 - 6.0 µm
3.0 - 6.0 µm
Average Particle Size/Laser Diffraction D50