Material Notes:
Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase bonding of refractory ceramic oxides and glass-ceramics for substrates.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 2.37 g/cc
0.0856 lb/in³
Particle Size 3.0 µm
3.0 µm
50% of particles
<= 25 µm
<= 25 µm
Thermal Properties Metric English Comments
CTE, linear 4.85 µm/m-°C
2.69 µin/in-°F
at Set Pt.
4.55 µm/m-°C

@Temperature 260 °C
2.53 µin/in-°F

@Temperature 500 °F
Softening Point 750 °C
1380 °F
Transformation Temperature 645 °C
1190 °F
Processing Properties Metric English Comments
Processing Temperature 900 °C
1650 °F
Typical Firing Temperature